欢迎登录材料期刊网

材料期刊网

高级检索

  • 论文(11)
  • 图书()
  • 专利()
  • 新闻()

THE EFFECT OF SILICON ADDITIVE ON THE STRUCTURE AND PROPERTIES OF C-B_4C-SiC COMPOSITE

HUANG Qizhong , YANG Qzaoqin and WU Lijun(Powder Metallurgy Research institute , Central Sonth University of Technology , Changsha 410083 , China Materials Research and Test Center , Hnnan University , Changsha 410082 , ChinaLab. of Atomic Imaging of Solids , Institute of Metal Research , Chinese Academy of Sciences , Shenyang110015 , ChinaState Key Laboratory for Corrosion and Protection , Institute of Corrosion and Protection of Metals , Chinese Academy of Sciences , Shenyang 110015 , China)Manuscript received 4 August 1995 , in revised form 6 April 1996

金属学报(英文版)

A Preliminary study of the effect of silicon additive on the structure and properites of C-B_4C-SiC composite was conducted. A liquid Phase has formed and the liquid Si reacts with C to form SiC at the grain boundary when sintering, which accelerates the sintering process and retards the grain growth. Consequently, the density and strength of the composite increase markedly. And the increase in the density increases the oxidation resistance and decreases the specific resistance of the composite. Furthermore,the C-B_4 C-SiC composite has good heat-shock resistance. The phenomena may be dueto the strengthening and toughening of microcracks.

关键词: :Si additive , null , null

A MODEL FOR THE ACTIVITY COEFFICIENTS OF WATER IN THE AQUEOUS SOLUTION OF HCl-MCl_n (M=Ni, Cu, Na AND Fe) WITH CONSTANT CONCENTRATION RATIO XHCl/XMCl_n

Q.R. Zhang , Y.G. Li and Z. Fang (Department of Chemistry , Central South University of Technology , Changsha 410083 , China)(Department of Chemistry , Central South University of Technology , Changsha 410083 , China)(Department of Chemistry , Central South University of Technology , Changsha 410083 , China)

金属学报(英文版)

In orber to calculate the activity coefficients of water in the aqueous solution systems of double electrolytes, HCl and MCln (M=Ni, Cu,Na and Fe), a simplified regular solution model has been derived based on the assumption that the electrolytes in the aqueous solution are treated as independent particles instead of their ion forms, and that the interaction of the component pair HCl-MCln in the aqueous solution is very weak as compared with the component pairs HCl-H2O and H2 O-MCln. The interchange energies of the component pairs in the discussed systems, ωWCl-H2o, ωH2o-NiCl2,ωH2o-CuCl2, ωH2o-NaCl and ωH2O-FeCl3, have been evaluated from the experimental data to be-69800, -212600, -90550, -42450 and -198310J·mol-1.

关键词: solution model; interchange energy; electrolyte solution

THE EXTRACTED COMPLEX FORMED BY MONO (2-ETHYLHEXYL)-2-ETHYLHEXYL PHOSPHATE WITH DIVALENT Mn

HUANG Kelong , SHU Wanyin , DING Dunhuang , LIU Guogen , DONG Ping , Central South University of Technology , Changsha , China HUANG Kelong , Lecturer , Department of Chemistry , Central South University of Technology , Changsha 410083 , China

金属学报(英文版)

In order to clarify the mechanism and the complex formed in the extraction of divalent Mn by alkylphosphonic acid monoester, the solid complex has been prepared by mono (2-ethylhexyl)-2-ethylhexyl phosphate, HEH(EH)P, HA with divalent Mn. The elemental analysis, magnetic susceptibility and thermogravimetry have been determined for the solid complex of HEH(EH)P-Mn(II) and the infrared spectrum has been carried out in comparison to the extractant HEH(EH)P. The extracted compound has also been studied by electronic and electron spin resonance spectroscopy in octane solvent and solid state at room temperature. On the basis of the measurements, it is concluded that the structure of the solid polymeric species MnA_2 is in a tetrahedral arrangement.

关键词: solvent extraction mono (2-ethylhexyl)-2-ethylhexyl phosphate , null , null

FRACTURE MECHANICS ANALYSIS OF THERMAL STRAIN FATIGUE LIFE FOR THE SINTERING MACHINE PALLET

LI Zhenzi and LI Ming (Department of Architectnre Engineering , Central South University of Technology , Changsha 410083 , China)LIAO Fuchang (Shenzhen School of Technology , Shenzhen 518029 , China)Manuscript received 10 August 1995 , in revised form 12 April 1996

金属学报(英文版)

In recent years elastic-plastic fracture mechanics has developed rapidly and is widely used to solve various engineering problems. The application of elastic-plastic fracture mechanics on the pallet of sintering machine is approached in detail for the first time in the present study. The theoretical results were compared with the actual data determined from sintering machine pallet. Results show that good agreement was achieved between the method suggested by the author and the actual data. The basis of determining design of the sintering machine pallet in iron and steel engineering has been provided and it will result in great economic benefits.

关键词: : pallet , null , null , null

A Simplified Regular Solution Model for Solubility of Nonmetal (2) in Metal(1)-Metal(3) Alloy Systems

Zheng FANG(Dept. of Chemistry , Central South University of Technology , Changsha 410083 , China)Quanru ZHANG(Dept. of Metallurgy , Changsha Technical College , Changsha 410012 , China)

材料科学技术(英)

A simplifled regular solution model for the solubility of nonmetallic element (2) in metal(1)-metal(3) alloy system has been derived and applied to the Fe-C-j, Ni-C-j and Fe-N-j (j denotes a metal) systems with satisfaction. The exchange energies of concerned systems are evaluated

关键词:

SYNTHESIS AND IDENTIFICATION OF CONDUCTING POLYANILINE DOPED WITH RARE EARTH CHLORIDE

C.M. Yang , Q.R. Zhang and Z. Fang(Department of Chemistry , Central South University of TecHnology , Changsha 410083 , China)

金属学报(英文版)

Polyaniline doped with rare earth chloride was synthcsized in organic solvent and identified by clemental analysis and ithered spectroscopy. The experimental results show that there exist both doping and complexation at the same time in the resulting product. When pH<4, prototnic acid doping is predominating, whereas rare earth ion complexation is predominating when pH>1. Moreover, polyanitine doped wih rare earth chloride exhibits better thermal stability than that doped with hydrochloric acid.

关键词: dope , null , null , null

AMORPHIZATION TRANSFORMATION BY MECHANICAL ALLOYING IN THE Mo-Si SYSTEM

M.W. Li , R.Z. Tang and W.X. Li (Department of Materials Science and Engineering , Central South University of Technology , Changsha 410083 , China)

金属学报(英文版)

Starting from elemental powders, complete MoSi2 powder forms abruptly between 3.5and 4 h during mechanical alloying (MA) of the Mo-66 at.% Si powders. Continuous milling of this MoSi2 Phase leads to a nanocrystalline powder and amorphizationtransformation takes place after 100 h milling. Howeven MA of the Mo-37.5 at.%Si powders does not result in the formation of the Mo5Si3 crystalline phase, but the formation of a Mo(Si) supersaturated solid solution (SSS) and a completely amorphots phase after 5 h and 70 h milling, respectively. The free energy of the Mo-Sisystem has been calculated and it has been found that there is no driving force for the amorphization reaction under normal conditions. The amorphization by MA of the Mo-Si system is attributed to a solid-state amorphization reaction in which defects and a very fine grain size induced during milling process may raise the free energy of the crystalline intermetallic phase (for MoSi2) or the Mo(Si) supersaturated solid solution (for Mo5Si3) above that of the amorphous phase.

关键词: mechanical alloying , null , null

DEVELOPMENT OF CONSTITUTE EQUATIONS FOR Ti-6Al-4V ALLOY UNDER HOT-WORKING CONDITION

L. X. Li and D. S. Peng (Department of Materials Science and Engineering , Central SouthUniversity of Technology , Changsha 410083 , China)

金属学报(英文版)

The deformaton behavior of Ti - 6Al - 4V alloy under hot - working condition has been studied by compression testing in the temperature range 750 - 950℃ and strain rate range 0.05 - 15s -1. The flow stress decreases with the increase of temperature and with the decrease of strain rate. After a steep initial strain hardening, a flow softening occurs. This softening is mainly ascribed to the temperature rise and dynamic recmptallisation.By a simple extension, a classical sinushyperbolic constitutive equation can be used to describe the flow behavior of Ti - 6Al - 4V alloy. flow stress is described as a function of strain, strain rate and temperature. The parameters Q, n andaare the same at differ- ent deformation conditions, and A is a funciton of strain.

关键词: Ti-6Al-4V alloy , null , null

EVOLUTION OF MICROSTRUCTURES AND HARDNESS DURING CONTINUOUS THERMO-MECHANICAL PROCESSING OF 6201 ALUMINUM ALLOY

H. Zhang , Y. Y. Liu , D. S. Peng and C. K. Wang (Department of Materials Science and Engineering , Central South University of Technology , Changsha 410083 , China)

金属学报(英文版)

Continuous thermo-mechanical processing (CTMP) of 6201 aluminum alloy was simulated on Gleeble-1500. The deformed specimens were analyzed by the observation of TEM and the measurement of hardness. It was shown that rapid solid solution and aging treatment can be effectively combined in one procedure by the strain induced during CTMP. The deformation temperature is ranging from 540* C to 300* C, the hardness increases directly before the 6th pass followed by a slight drop, the amount of precipitates increases with the holding time after deformation. Uniformly distributed and stabilized Mg2Si precipitates, as well as dislocation substructure can be observed on deformed specimens which have been subsequently held at 300℃ for 60 seconds.

关键词: 6201 aluminum alloy , null , null , null , null

INVESTIGATION OF MULTI-STEP THERMO-MECHANICAL TREATMENT OF CAN-FORGED TiAl-BASED ALLOY

Y.H. He , B. Y. Huang , Y. Liu and Y.X. Liu (Powder Metallurgy Research Institute , Central South University of Technology , Changsha 410083 , China)

金属学报(英文版)

The effects of a new technology, multi-step thermo-mechanical treatment, on the microstructure, deformation substructure and mechanical properties at ambient and elevated tempemture of can-forged Ti-33 Al-3 Cr-0.5Mo (wt%) Alloy were investigated.The results show that, after multi-step thermo-mechanical treatment of can-forged specimens, homogeneous, fine microstructures can be obtained in the whole TiAl-based alloy specimens. Furthermore, the specimen with homogeneous and fine full lamellae microstructure demonstrutes excellent comprehensive mechanical properties at ambient and elevated temperature.

关键词: TiAl-based alloy , null , null

  • 首页
  • 上一页
  • 1
  • 2
  • 下一页
  • 末页
  • 共2页
  • 跳转 Go

出版年份

刊物分类

相关作者

相关热词